Introduction to Recrystallized Silicon Carbide (RSiC)

Recrystallized SiC refers to the transmission and migration of atoms through surface diffusion and evaporation-condensation mechanism at high temperatures (2100~2300℃) so that the SiC blank is sintered to obtain strength. This is due to the difference in vapor pressure between the convex (positive) and concave (negative) curvatures, which causes small-sized SiC particles to evaporate first and then preferentially deposit on the near-neck surface of larger SiC particles, that is, the material evaporated from the small grains with convex surfaces condenses on the grains with concave and flat surfaces, so that the neck of the large grain grows, the small grains are consumed to disappear, and the SiC grains are directly combined to obtain strength. The high-temperature sintering of recrystallized SiC is usually carried out in a graphite induction furnace. Recrystallization begins at 1900℃ due to particle surface diffusion, and the sintering temperature for maximum strength is 2150~2300℃.

Recrystallized SiC has the following characteristics:

1 Because there is no grain boundary or volume diffusion during the sintering process, and the evaporation condensation and surface diffusion do not reduce the distance between SiC particles, there is almost no volume shrinkage during the sintering process;

2 Recrystallized SiC blanks have almost no density increase after sintering. The initial blank microstructure determines the performance of the final product, which requires the blank to have a high density. Therefore, SiC powder grading and the appropriate molding process are two key links in the preparation of recrystallized SiC. Generally, a mixture of SiC particles with bimodal distribution is used to increase the bulk density. Slip casting is better than cold isostatic pressing and extrusion molding. It can obtain a higher volume density (about 2.7g/cm3) and can form large-sized and complex-shaped recrystallized SiC parts. The method of molding with the help of paraffin wax is best not to use because it will contain residual carbon after wax removal;

3 Recrystallized SiC has very clear and clean grain boundaries and does not contain glass phases and impurities because any oxides or metal impurities have been volatilized at high temperatures of 2150~2300℃;

4 The recrystallized SiC products after sintering contain 20%~30% residual porosity.

Recrystallized SiC does not contain any metal phase or glass liquid phase, and has a high porosity (20%~30%), so it has excellent high-temperature resistance and thermal shock resistance; coupled with its good high-temperature thermal conductivity, it is an ideal candidate material for high temperature kiln furniture, heat exchangers or combustion nozzles, because these applications emphasize not high strength, high toughness and high hardness, but thermal shock resistance and high temperature thermal conductivity.

Edgetech specializes in the manufacture and sale of advanced ceramic parts. We provide customized production and high-precision processing for a variety of high-performance ceramic materials, including alumina ceramics, zirconium oxide ceramics, silicon nitride, silicon carbide, boron nitride, aluminum nitride, etc. Our ceramic parts can be found in many industries, such as machinery, chemistry, medicine, semiconductors, vehicles, electronics, metallurgy, etc.